氧化铝空心球砖主要是以氧化铝空心球为主要原料,以刚玉细粉做添加物,在高温1800度窑炉内烧制而成。它具有抗高温,热稳定性好,保温效果优良等特点。近年来广泛用于高温推板电窑、遂道窑、梭式窑炉等各种高温工业窑炉高温区域。使用效果持久耐用,为企业创造了经济效益。 |
项目Ltem | 氧化铝空心球砖 Alumina bubble brick | 氧化锆空心球砖Zirconia bubble brick | ||||
| 85砖 | 87砖 | 90砖 | 95砖 | 99砖 | 98砖 |
AL2O3% | ≥85 | ≥87 | ≥90 | ≥95 | ≥99 | - |
ZrO2% | - | - | - | - | - | ≥98(含稳定剂) |
SiO2% | ≤13 | ≤12 | ≤8 | ≤4 | ≤0.2 | ≤0.2 |
Fe2O3% | ≤0.3 | ≤0.2 | ≤0.2 | ≤0.2 | ≤0.2 | ≤0.2 |
体积密度g/cm3 Bulk density | 1.2-1.7 | 1.3-1.5 | 1.4-1.7 | 1.4-1.7 | 1.4-1.7 | 2.5-3.5 |
常温耐压强度MPa Cold crushing strength | ≥12 | ≥10 | ≥10 | ≥10 | ≥9 | ≥8 |
荷重软化开始温度℃(0.1MPa ,0.6%) Refractoriness under load | ≥1650 | ≥1650 | ≥1700 | ≥1700 | ≥1700 | ≥1700 |
重烧线变化率%(1600℃x3h) Reheating linear change | ±0.3 | ±0.3 | ±0.3 | ±0.3 | ±0.3 | ±0.2 |
热膨胀系数x10-6(室温-1300℃) Thermal expansion coefficient | ~7.8 | ~7.8 | ~8.0 | ~8.0 | ~8.6 | ~9.1 |
导热系数 w/(m.k)(平均温度800℃) Thermal Conductivity
| ≤0.8 | ≤0.8 | ≤1.3 | ≤1.4 | ≤1.5 | ≤0.3 |
**使用温度℃ Max service temperature | 1680 | 1700 | 1700 | 1700 | 1800 | 2200 |
免责声明:当前页为 赛隆 氧化铝空心球砖 隔热保温系列优良耐火砖产品信息展示页,该页所展示的 赛隆 氧化铝空心球砖 隔热保温系列优良耐火砖产品信息及价格等相关信息均有企业自行发布与提供, 赛隆 氧化铝空心球砖 隔热保温系列优良耐火砖产品真实性、准确性、合法性由店铺所有企业完全负责。世界工厂网对此不承担任何保证责任,亦不涉及用户间因交易而产生的法律关系及法律纠纷,纠纷由会员自行协商解决。
友情提醒:世界工厂网仅作为用户寻找交易对象,就货物和服务的交易进行协商,以及获取各类与贸易相关的服务信息的渠道。为避免产生购买风险,建议您在购买相关产品前务必确认供应商资质及产品质量。过低的价格、夸张的描述、私人银行账户等都有可能是虚假信息,请您谨慎对待,谨防欺诈,对于任何付款行为请您慎重抉择。
投诉方式:fawu@gongchang.com是处理侵权投诉的专用邮箱,在您的合法权益受到侵害时,请将您真实身份信息及受到侵权的初步证据发送到该邮箱,我们会在5个工作日内给您答复,感谢您对世界工厂网的关注与支持!
电话18703867334
手机18703867334
QQ839961814